# Corrosion under insulation (CUI), explained

> Corrosion under insulation (CUI) happens when water gets past damaged cladding and the insulation holds it against the steel, so wall loss can grow out of sight until a leak. This film shows where the water comes from, why heat and shutdowns matter, and how inspectors find it.

- Label: Fact
- Type: Video
- Published: 2026-11-19T19:43:44+09:00
- By: Jiakai Yang
- Researched and drafted by: Beacon's AI newsroom
- Checked by: Jiakai Yang on 2026-11-24
- Topics: Refining, Upstream and offshore
- Canonical: https://beaconnews.winda.ai/videos/corrosion-under-insulation/

Insulation keeps the heat in. It can also hold water against the steel, out of sight. This is corrosion under insulation, or CUI.[2][1]

Water comes from rain, sprinkler systems, cooling towers or condensation, and gets in wherever the cladding fails: a failed joint seal, a dent, a panel not refitted after maintenance.[3][2]

Inside, it runs to the low points. In the field, damage is often found at the six o'clock position.[2][3]

Fibrous insulation, such as mineral wool, soaks it up and holds it against the metal, with air close by.[2]

That is all steel needs. At an anode, iron leaves the metal and gives up electrons. They travel through the wall to a cathode, where oxygen and water consume them.[4]

Heat keeps it going. In 2011 the UK safety regulator rated thirty to a hundred and twenty degrees Celsius the most critical range; older pipework was at risk even when cold, and shutdowns put hot lines back at risk.[2]

And under the cladding, wall loss can grow unseen until a leak.[2][1]

So inspectors cut small windows where damage is most likely, or screen through the insulation with pulsed eddy current, guided waves or radiography.[2][3][5]

Offshore, in 2018, exhaust piping under insulation blankets was found corroded through.[6]

Corrosion under insulation. Read more in the Beacon Library.[2]

## Sources

1. [2025 Publications Catalog, entry for RP 583, Corrosion Under Insulation and Fireproofing (scope as API describes it), American Petroleum Institute (API)](https://www.api.org/-/media/files/publications/2025-catalog/2025_pubs%20catalog.pdf)
2. [Corrosion under insulation of plant and pipework, semi-permanent circular SPC/TECH/GEN/18, issued 1 March 2011 (archived copy; the live page no longer exists), UK Health and Safety Executive](https://web.archive.org/web/20210123065144/https://www.hse.gov.uk/foi/internalops/hid_circs/technical_general/spc_tech_gen_18.htm), 2011-03-01
3. [Cao, Pojtanabuntoeng, Esmaily, Thomas, Brameld, Amer and Birbilis, A Review of Corrosion under Insulation: A Critical Issue in the Oil and Gas Industry, Metals 12(4), 561, 2022, Metals (MDPI), via MIT DSpace](https://dspace.mit.edu/handle/1721.1/141822.2), 2022-03-25
4. [Forms of Corrosion, NASA Kennedy Space Center, Corrosion Engineering Laboratory](https://public.ksc.nasa.gov/corrosion/forms-of-corrosion/)
5. [Cawley, Guided waves in long range nondestructive testing and structural health monitoring: principles, history of applications and prospects, NDT & E International 142, 103026, 2024, NDT & E International (open access, CC BY 4.0)](https://www.ndt.net/article/ndt-e-intl/papers/1-s2.0-S0963869523002414-main.pdf), 2023-12-22
6. [Safety Bulletin No. 013: Severe Corrosion Found Under Insulation, Bureau of Safety and Environmental Enforcement](https://www.bsee.gov/sites/bsee.gov/files/safety-bulletin-013-corrosion-under-insulation.pdf), 2018-12-03

Published by Winda Beacon (https://beaconnews.winda.ai).